Not known Facts About znse
Structural Evaluation point out the films exhibited cubic favored orientation alongside the plane (111) plus the crystallinity and crystallite measurement of films increases linearly with film thickness. The optical band hole ranges from 2.69 to 2.eighty one eV and it's Established that it improves with film thickness. According to the used Swanepo